Customer Equipment Substrate Environment Date of application
Prague Incinerator Plant Superheater CS Clinkering, Ash Abrasion, Abrasion Sept 2024
Prague Incinerator Plant Hopper ARC Clinkering, Abrasion 700 oC/1,292 oF Sept 2024
Pyrotek Blansko Gas kiln PYR Energy savings Jun 2023
Power Stations Opatovice K4 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF Dec 2022
Power Stations Opatovice K4 Superheater II tubes CS Ash Abrasion, 700 oC/1,292 oF Nov 2022
Power Stations Opatovice K4 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF Nov 2022
PRECHEZA Prerov Burner of calcination furnace in Iron Pigments Production CH Lifetime Oct 2022
PRECHEZA Prerov Burner of dehydratation furnace in Iron Pigments Production CH Lifetime Oct 2022
CEZ PS Porici via Martia plc FK8 Walerwall in CC CS Ash Abrasion Oct 2022
Power Stations Opatovice K3 ECO II tubes CS Ash Abrasion, 700 oC/1,292 oF Oct 2022
Power Stations Opatovice K3 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF Sept 2022
Power Stations Opatovice K3 Superheater II tubes CS Ash Abrasion, 700 oC/1,292 oF Sept 2022
CEZ PS Melnik via Energotrans plc K6 Boiling tubes&Bottom part of superheater 3 Cr/Mo Ash Abrasion, 750 oC/1,390 oF Sept 2022
Power Stations Opatovice K3 Waterwall around urea nozzles CS Corrosion by urea, 700 oC/1,292 oF Sept 2022
Power Stations Opatovice K3 ECO II U-bends CS Ash Abrasion, 700 oC/1,292 oF Aug 2022
Power Stations Opatovice K6 ECO II Hanger tubes CS Ash Abrasion, 700 oC/1,292 oF July 2022
CEZ PS Porici via Martia plc FK8 Walerwall in CC CS Ash Abrasion Jun 2022
Power Stations Opatovice K6 CC Walerwall tubes (rear part) CS Ash Abrasion, 700 oC/1,292 oF Jun 2022
Power Stations Opatovice K5 Superheater tubes CS Ash Abrasion, 700 oC/1,292 oF Jun 2022
CEZ PS Ledvice via Power Industry K6 Flueduct CS Ash Abrasion, 400 oC/752 oF May 2022
Power Stations Opatovice K2 Superheater tubes CS Ash Abrasion, 700 oC/1,292 oF May 2022
Power Stations Opatovice K2 Waterwall around urea nozzles CS Corrosion by urea, 700 oC/1,292 oF May 2022
Power Stations Opatovice K2 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF May 2022
PRECHEZA Prerov H2SO4 Plant S1 Stack CS Corrosion by acidic condensates of SO2 Oct 2021
PRECHEZA Prerov Burner of dehydratation furnace in Iron Pigments Production CH Lifetime Oct 2021
CEZ PS Ledvice via Power Industry FK4 Walerwall in CC CS Abrasion&Corrosion 870oC/1,600F Sept 2021
CEZ PS Porici via Martia plc FK8 Walerwall in CC CS Ash Abrasion Sept 2021
SEV.EN EC via SES Tlmace plc K2 Avoiding tubes around burners + ECO U-bends CS Ash Abrasion, 700 oC/1,292 oF Sept 2021
Power Stations Opatovice K5 ECO II Tubes CS Ash Abrasion, 700 oC/1,292 oF Aug 2021
Power Stations Opatovice K5 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF Aug 2021
Power Stations Opatovice K5 Waterwall around urea nozzles CS Corrosion by urea, 700 oC/1,292 oF Aug 2021
CEZ PS Porici via Martia plc FK 7 - LUVO Tubes ("cold" side) CS Corrosion by acidic condensate, 140oC/284F Aug 2021
Power Stations Opatovice K6 Hopper bends in CC CS Ash Abrasion, 700 oC/1,292 oF June 2021
Power Stations Opatovice K6 Waterwall around urea nozzles CS Corrosion by urea, 700 oC/1,292 oF June 2021
CEZ PS Ledvice via Power Industry K6 Flueduct CS Ash Abrasion, 400 oC/752 oF June 2021
Power Stations Opatovice K6 ECO II Tubes CS Ash Abrasion, 700 oC/1,292 oF June 2021
Power Stations Opatovice K5 Superheater tubes CS Ash Abrasion, 700 oC/1,292 oF June 2021
CEZ PS Melnik K10 Water walls in CC Cr/Mo Abrasion&Corrosion 870oC/1,600F May 2021
Power Stations Opatovice K5 ECO II U-bends CS Abrasion May 2021
Power Stations Opatovice Mixing centre, settling tank OZS1A CS Wet slag abrasioin at ambient temperature Apr 2021
Power Stations Opatovice K2 Hopper bends in CC CS Abrasion Apr 2021
Power Stations Opatovice K3 Hopper bends in CC CS Abrasion Apr 2021
Power Stations Opatovice K1 Hopper bends in CC CS Abrasion Oct 2020
Power Stations Opatovice K4 Hopper bends in CC CS Abrasion Oct 2020
CEZ PS Melnik via Power Industry plc B9 Flueduct CS Corrosion by undesulfirised flue gas under dew point Sept 2020
MVV Umwelt, Königs Wusterhausen, Germany Wood chips boiler CS Corrosion and clinkering Sept 2020
Power Stations Opatovice K2 Hopper bends in CC CS Abrasion Aug 2020
Power Stations Opatovice K2 Superheater tubes CS Ash Abrasion, 700 oC/1,292 oF Aug 2020
SEV.EN EC via EDMS Pezinok Blades of 5 axial fans CS Ash Abrasion, 200 oC/392 oF Aug 2020
CEZ PS Porici via Martia plc FK8 Water walls in CC CS Ash Abrasion Aug 2020
Pilsen Heating Comp plc K3 Ceiling&surroudings of burners CS c Aug 2020
CEZ PS Melnik via Power Industry plc K6 Flueduct CS Corrosion by undesulfirised flue gas under dew point Aug 2020
CEZ PS Tusimice Boiler D Evaporator water wall Cr/Mo High Temperature Corrosion & Abrasion, 1,050oC/1,924oF July 2020
CEZ PS Tusimice Boiler C Evaporator water wall Cr/Mo High Temperature Corrosion & Abrasion, 1,050oC/1,924oF July 2020
CEZ PS Ledvice via Power Industry K6 Flueduct CS Abrasion and Corrosion 180 oC / 355 oF July 2020
CEZ PS Porici via Martia plc LUVO Tubes ("cold" side) CS Corrosion by acidic condensate, 140oC/284F July 2020
Power Stations Opatovice K5 ECO II hung tubes CS Abrasion June 2020
Power Stations Opatovice K6 ECO II hung tubes CS Abrasion June 2020
Power Stations Opatovice K6 Hopper bends in CC CS Abrasion June 2020
Power Stations Opatovice K5 Hopper bends in CC CS Abrasion June 2020
Power Stations Opatovice K3  Hopper bends in CC CS Abrasion May 2020
Power Stations Opatovice K2 ECO II U-bends CS Abrasion Apr 2020
CEZ PS Prunerov K24 Evaporator in CC Cr/Mo Corrosion and abrasion Apr 2020
CEZ PS Prunerov K24  Hopper in CC LAS Abrasion Apr 2020
MVV Umwelt Dundee. Scotland, GB Water wall and plate superheater CS Corrosion and clinkering Oct 2019
CEZ PS Porici via Protis Ing. Ostrava plc FK8 LUVO Tubes ("cold" side) CS Corrosion by acidic condensate, 140oC/284F Sept 2019
PRECHEZA Prerov Burner of dehydratation furnace in Iron Pigments Production CH Lifetime Sept 2019
PRECHEZA Prerov Burner of calcination furnace in Iron Pigments Production CH Lifetime Sept 2019
CEZ PS Tusimice Block B Evaporator in CC Cr/Mo Corrosion and abrasion Aug 2019
TEREOS TTD plc Water heaters of coal boilers CS Corrosion July 2019
CEZ PS Melnik via Power Industry K5 ECO I Tubes&U-bends CS Ash abrasion July 2019
CEZ PS Tusimice Block A Evaporator in CC Cr/Mo Corrosion and abrasion July 2019
CEZ PS Melnik via G-TeamProgres K6 Superheater II&IV tubes Cr/Mo Corrosion under deposits, 600oC/1,112F July 2019
CEZ PS Melnik via G-TeamProgres K5 Superheater II&IV tubes Cr/Mo Corrosion under deposits, 600oC/1,112F July 2019
CEZ PS Melnik via G-TeamProgres K4 Superheater II&IV tubes Cr/Mo Corrosion under deposits, 600oC/1,112F July 2019
CEZ PS Porici via Martia plc LUVO Tubes ("cold" side) CS Corrosion by acidic condensate, 140oC/284F July 2019
Power Stations Opatovice K6 Crude fuel bunker CS Coal arching, clinkering June 2019
CEZ PS Prunerov K23 Evaporator in CC Cr/Mo Corrosion and abrasion May 2019
CEZ PS Prunerov K23  Hopper in CC LAS Abrasion May 2019
Power Stations Opatovice K6 ECO II tubes CS Abrasion Apr 2019
PRECHEZA Prerov Burners chamber of dehydratation furnace in Iron Pigments Production CH Lifetime Apr 2019
PRECHEZA Prerov Burners chamber of calcination furnace in Iron Pigments Production Ch Lifetime Apr 2019
Energy centre Ltd Jidrichuv Hradec K5 Superheater tubes Cr/Mo Clinkering Mar 2019
CEZ PS Ledvice via UniSteel Ltd Tubes LUVO LAS Corrosion 180 oC/355 oF Mar 2019
MVV Umwelt, Königs Wusterhausen, Germany Wood chips boiler CS Corrosion & Clinkering Mar 2019
Meduna Vacuum Quenching Plant Ltd Spacing plates G Lifetime Feb 2019
CEZ PS Prunerov K25 Evaporator in CC Cr/Mo Corrosion Feb 2019
CEZ PS Prunerov K25  Hopper in CC LAS Abrasion Feb 2019
Meduna Vacuum Quenching Plant Ltd Spacing plates G Lifetime Jan 2019

 

Customer Equipment Substrate Environment Date of application
PRECHEZA Prerov Burners chamber of dehydratation furnace in Iron Pigments Production CH Lifetime Sept 2018
CEZ PS Melnik K2 Burners 21-24 surrounding CS Clinkering Sept 2018
CEZ PS Melnik K1 Burners 11-14 surrounding CS Clinkering Sept 2018
CEZ PS Melnik K3 Burners 31-34 surrounding CS Clinkering Sept 2018
CEZ PS Porici K1&K2&K3 Superheaters II&IV tubes Cr/Mo Clinkering Sept 2018
Power Stations Opatovice K4 ECO II tubes CS Abrasion Sept 2018
Power Stations Opatovice K4 Superheater IV tubes Cr/Mo Clinkering Aug 2018
CEZ PS Tusimice Boilers C+D waterwalls in CC at tercial air inlets Cr/Mo Abrasion Aug 2018
Power Stations Opatovice K4 Hopper bends in CC CS Abrasion Aug 2018
CEZ PS Porici FK7 Walls of electrostatic dust separator CS Corrosion Aug 2018
CEZ PS Tusimice Boilers A+B waterwalls in CC at tercial air inlets Cr/Mo Abrasion Aug 2018
CEZ PS Porici FK7 Walls of electrostatic dust separator CS Corrosion July 2018
Power Stations Opatovice K6 Hopper bends in CC CS Abrasion July 2018
Power Stations Opatovice K5 Hopper bends in CC CS Abrasion July 2018
Power Stations Opatovice K1 Hopper bends in CC CS Abrasion June 2018
Power Stations Opatovice K2 Hopper bends in CC CS Abrasion June 2018
Power Stations Opatovice K1 Superheater IV tubes CS Clinkering June 2018
Power Stations Opatovice K3 Hopper in CC CS Abrasion May 2018
Pilsen Heating Comp plc K7 superheater plate Cr/Mo Clinkering May 2018
MVV Umwelt, Königs Wusterhausen, Germany Wood chips boiler CS Corrosion & Clinkering March 2018

 

Customer Equipment Substrate Environment Date of application
SEVEN.EC K4 Hopper CC CS Ash Abrasion, 700 oC/1,292 oF Dec 2017
CEZ Power Station Melnik via TERMONTA PRAHA K6 Burners surroundings CS Clinkering Sept 2017
PRECHEZA Prerov Burners chamber of dehydratation furnace in Iron Pigments Production CH Lifetime Sept 2017
PRECHEZA Prerov Burners chamber of calcination furnace in Iron Pigments Production CH Lifetime Sept 2017
Power Stations Opatovice K1 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF Sept 2017
Power Stations Opatovice K1 ECO II tubes CS Ash Abrasion, 700 oC/1,292 oF Sept 2017
Power Stations Opatovice K2 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF Sept 2017
SEVEN.EC Chvaletice K1 ECO tubes CS Ash Abrasion, 700 oC/1,292 oF Aug 2017
Pilsen heating station Burners surroundings CS Clinkering Aug 2017
CEZ Power Station Melnik via TERMONTA PRAHA K5 Burners surroundings CH Clinkering Aug 2017
Power Stations Opatovice K1 U-bends ECO II CS Ash Abrasion, 700 oC/1,292 oF Aug 2017
CEZ PS Tusimice Bloc A Hopper CC CS Ash Abrasion, 700 oC/1,292 oF Aug 2017
CEZ PS Tusimice Bloc B Hopper CC CS Ash Abrasion, 700 oC/1,292 oF Aug 2017
PS Tisova K11 Combustig Chamber LAS Abrasion, 950 oC/1,742 oF Aug 2017
CEZ Power Station Melnik via Power Industry K11 Hopper CC CS Ash Abrasion, 700 oC/1,292 oF July 2017
Power Stations Opatovice K3 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF July 2017
CEZ PS Porici via G-Team FK 7 Superheater tubes - corrosion protection Cr/Mo Corrosion under deposits, 600 oC/1,112 oF July 2017
Power Stations Opatovice K4 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF June 2017
MVV Umwelt, Königs Wusterhausen, Germany Wood chips boiler CS Corrosion & Clinkering June 2017
Power Stations Opatovice K5 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF May 2017
Power Stations Opatovice K6 Hopper U-bends CS Ash Abrasion, 700 oC/1,292 oF May 2017
Power Stations Opatovice K4 U-bends ECO CS Ash Abrasion, 700 oC/1,292 oF Apr 2017
PRECHEZA Prerov Burners chamber of dehydratation furnace in Iron Pigments Production CH Lifetime Apr 2017
PRECHEZA Prerov Burners chamber of calcination furnace in Iron Pigments Production CH Lifetime Apr 2017
SEVEN.EC via KP Ria K4 Cowlings of powder burners CS Clinkering, 420 oC/788 oF Jan 2017

 

 

Customer Equipment Substrate Environment Date of application
SEVEN.EC K1 lower ECO back wall CS Ash abrasion, 360oC/680F Oct 2016
PRECHEZA Burners chamber in dehydration furnace producing iron pigments CH Lifetime increasing Oct 2016
PRECHEZA Burners chamber in calciner producing iron pigments CH Lifetime increasing Oct 2016
SEVEN.EC via KP Ria K3 cowlings of powder burners CS Clinkering, 420oC/788F Oct 2016
CEZ PS Porici via G-Team FK 7 Superheater tubes - corrosion protection Cr/Mo Corrosion under deposits, 600oC/1,112F Oct 2016
Power Stations Opatovice K4 Superheater PP II Cr/Mo Clinkering Sept 2016
Power Stations Opatovice K4 Hopper U-bends CS Ash abrasion, 700oC/1,292F Sept 2016
Power Stations Opatovice ECO II K5 suspension tubes CS Abrasion Sept 2016
Power Stations Opatovice ECO II K6 suspension tubes CS Abrasion Sept 2016
Power Stations Opatovice via SES Tlmace K5 recycle pipeline CS Ash abrasion, 700oC/1,292F Aug 2016
Power Stations Opatovice via SES Tlmace K6 recycle pipeline CS Ash abrasion, 700oC/1,292F Aug 2016
Veoila Energy  - Heating Plant Prerov K2 burners RC Clinkering, 1,200oC/2,192F July 2016
Power Station Melnik via Energy Machinery K11 Evaporator Cr/Mo Clinkering, 950oC/1,742F July 2016
Power Stations Opatovice via SES Tlmace K3 recycle pipeline CS Ash abrasion, 700oC/1,292F June 2016
PRECHEZA Burners chamber in dehydration furnace producing iron pigments CH Lifetime increasing June 2016
CEZ PS Tisova FK1 Combusting chamber LAS Abrasion, 950oC/1,742F June 2016
Power Stations Opatovice via SES Tlmace K2 recycle pipeline CS Ash abrasion, 700oC/1,292F May 2016
Power Station Melnik via DIZ Bohemia K3 Tubes LUVO II CS Corrosion by acidic condensates, 140oC/284F Apr 2016
 UMICORE NV Metal Refinery Furnace   Off-gas system LAS High Temperature Corrosion & Abrasion, 800oC/1,472F Apr 2016
Power Stations Opatovice K6 Superheater PP IV Cr/Mo Clinkering, 1,000oC/1,832F Jan 2016
Power Stations Opatovice K6 Surrounding tubes of powder burners CS Clinkering, 1,200oC/2,192F Jan 2016

 

 

Customer Equipment Substrate Environment Date of application
Sev.en EC K3 Front hopper wall in CC CS Clinkering Dec 2015
Power Stations Opatovice via SES Tlmace K3 ECO II & hooks CS Ash abrasion, 700oC/1,292F Nov 2015
Power Stations Opatovice via SES Tlmace K3 hopper CS Ash abrasion, 700oC/1,292F Nov 2015
Sev.en EC K1 water wall CS Clinkering Nov 2015
PRECHEZA Burners chamber of dehydratation furnace in Iron Pigments Production CH Lifetime Nov 2015
Power Stations Opatovice via SES Tlmace K5 ECO II & hooks CS Abrasion Oct 2015
Power Stations Opatovice via SES Tlmace K5 hopper CS Ash abrasion, 700oC/1,292F Oct 2015
Power Stations Opatovice via SES Tlmace K2 ECO II & hooks CS Ash abrasion, 700oC/1,292F Oct 2015
Power Stations Opatovice via SES Tlmace K2 hopper CS Ash abrasion, 700oC/1,292F Oct 2015
CEZ PS Porici via DIZ Bohemia LUVO Tubes ("cold" side) CS Corrosion by acidic condensate, 140oC/284F Sept 2015
Power Station Melnik via Energy Machinery K9 Tubes & U-bends in lower part of Evaporator CS Ash abrasion, 700oC/1,292F Sept 2015
Power Stations Opatovice K5 U-bends ECO CS Ash abrasion, 700oC/1,292F Sept 2015
Power Stations Opatovice K3 U-bends ECO CS Ash abrasion, 700oC/1,292F Sept 2015
Power Stations Opatovice K2 U-bends ECO CS Ash abrasion, 700oC/1,292F Sept 2015
CEZ PS Tusimice via CEZ Energy Products Ash hopper CS Ash arching, 150oC/302F Sept 2015
Power Station Melnik via DIZ Bohemia K4 12 blocks of LUVO CS Abrasion, 450oC/842F Aug 2015
Power Station Melnik via Power Industry K10 Evaporator Tubes & U-bends CS Ash abrasion, 700oC/1,292F Aug 2015
Power Stations Opatovice via SES Tlmace K2 recycle pipeline CS Ash abrasion, 700oC/1,292F Aug 2015
Heating Plant Zilina via SES Tlmace K2 Burners RC Clinkering, 900oC/1,652F Aug 2015
Heating Plant Zilina via SES Tlmace K5 Burners RC Clinkering, 900oC/1,652F Aug 2015
Power Stations Opatovice K1 ECO U-bends CS Ash abrasion, 700oC/1,292F July 2015
Power Stations Opatovice via SES Tlmace K3 recycle pipeline CS Ash abrasion, 700oC/1,292F July 2015
Power Stations Opatovice via SES Tlmace K5 recycle pipeline CS Ash abrasion, 700oC/1,292F July 2015
Heating Plant Zilina via SES Tlmace K2 Schott superheaters Cr/Mo Abrasion, corrosion, deposits, 1,150oC/2,102F June 2015
Heating Plant Zilina via SES Tlmace K5 Schott superheaters & Wall tubes Cr/Mo Clinkering, corrosion, 1,150oC/2,102F June 2015
Power Stations Opatovice via SES Tlmace K3 ECO I CS Abrasion June 2015
Power Stations Opatovice Hopper K4 U-bends CS Ash abrasion, 700oC/1,292F June 2015
Power Stations Opatovice ECO II K6 suspension tubes CS Ash abrasion, 700oC/1,292F June 2015
Power Stations Opatovice via SES Tlmace K2 ECO I CS Abrasion June 2015
Power Station Tisova FK1 Combusting chamber LAS Abrasion, 950oC/1,742F May 2015
Power Stations Opatovice via SES Tlmace K5 ECO I CS Abrasion Apr 2015
Power Station Melnik via DIZ Bohemia K2 12 blocks of LUVO CS Abrasion, 450oC/842F March 2015
Power Stations Opatovice via SES Tlmace K6 ECO II CS Abrasion Jan 2015
Power Stations Opatovice via SES Tlmace Hopper K6 U-bends CS Ash abrasion, 700oC/1,292F Jan 2015
Heating Plant Zilina via SES Tlmace K1 Schott superheaters Cr/Mo Abrasion, corrosion, 1,150oC/2,102F Jan 2015
Heating Plant Zilina via SES Tlmace K1 coal dryers Cr/Mo Clinkering, corrosion, 1,150oC/2,102F Jan 2015

 

 

Customer Equipment Substrate Environment Date of application
Power Stations Opatovice via SES  Tlmace EOp K6 recirculation pipeline's parts CS Abrasion Dec 2014
Power Stations Opatovice K6 ECO II U-bends CS Abrasion Dec 2014
Power Stations Opatovice via SES Tlmace EOp K6 ECO I CS Abrasion Nov 2014
Power Station Porici FK8 membrane wall CS Abrasion Aug 2014
Pilsen heating station Burners CS Clinkering Aug 2014
Pilsen heating station Hopper CS Abrasion Aug 2014
Heating Plant Karviná via Vítkovice Power Engineering K3 smoke bar CS Corrosion Aug 2014
Power Station Tusimice K 1&2 Flue pipe CS Pitting corrosion, shock water spraying from 150oC to 5oC/from 302F to 41F July 2014
Power Station Tusimice K 1&2 Flue pipe - Checked after two years: 8% loss of original thickness only CS Pitting corrosion, shock water spraying from 150oC to 5oC/from 302F to 41F July 2016
EGT servis sro Recuperator SS Abrasion July 2014
Power Stations Opatovice Hopper K4 U-bends CS Ash Abrasion, 700oC/1,292F June 2014
Power Stations Opatovice ECO II K4 tubes CS Ash Abrasion, 700oC/1,292F June 2014
Power Stations Opatovice Hopper K5 U-bends CS Ash Abrasion, 700oC/1,292F June 2014
Power Station Tusimice K 3&4 Flue pipe CS Pitting corrosion, shock water spraying from 150oC to 5oC/from 302F to 41F June 2014
Power Stations Opatovice Hopper K1 U-bends CS Ash Abrasion, 700oC/1,292F May 2014
Power Stations Opatovice Hopper K2 U-bends CS Ash Abrasion, 700oC/1,292F May 2014
Power Stations Opatovice Hopper K3 U-bends CS Ash Abrasion, 700oC/1,292F May 2014
Power Stations Chvaletice K1 Lower ECO - back wall CS Ash Abrasion, 360oC/680F May 2014
Power Stations Opatovice K6 Superheater IV Tubes Cr/Mo Clinkering Nov 2014

 

Customer Equipment Substrate Environment Date of application
Kronospan Jihlava via DITHERM Combusting chamber's membrane wall CS Clinkering Dec 2013
MHKW, Ofenbach, Germany via GOSSLER TDM InsulRef Sp. z o.o Municipal wastes' Incinerator SiC Clinkering Oct 2013
CEZ HP Dvur Kralove Combustion chamber K1 Refractory Clinkering Sept 2013
CEZ PS Porici LUVO FK8 Tubes CS Corrosion by acidic condensates, 140oC/284F Aug 2013
CEZ Power Station Hodonin Tubes LUVO CS Low temperature corrosion due to condensation July 2013
Power Stations Opatovice K2 CC  hopper CS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice K3 CC hopper CS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice Space below CC hopper CS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice Space below CC hopper CS Ash Abrasion, 700oC/1,292F July 2013
United Energy Superheater Tubes (K9) Cr/Mo Abrasion from fluid bed 880oC/1,616F July 2013
CEZ Power Station Tisova Combusting chamber RC 950oC/1,742F July 2013
CEZ Power Station Tisova Cyclone RC Abrasion, 950oC/1,742F July 2013
CEZ Power Station Tisova Membrane wall LAS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice ECO II K1 tubes CS Ash Abrasion, 700oC/1,292F July 2013
Prague Incinerator Plant K2 Heatexchanger LUVO CS Corrosion by acidic condensates, 140oC/274F July 2013
EGT Servis Hradec Králové Recuperators SS Abrasion July 2013
Power Stations Opatovice Hopper K1 U-bends CS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice Space below CC nose CS Ash Abrasion, 700oC/1,292F July 2013
Power Stations Opatovice ECO K4 U-bends CS Ash Abrasion, 700oC/1,292F May 2013
Power Stations Opatovice K6 hopper CC - right side CS Ash Abrasion, 700oC/1,292F May 2013
Power Stations Opatovice Tubes ECO II (K6) CS Ash Abrasion, 700oC/1,292F May 2013
Power Stations Opatovice Space below CC hopper CS Ash Abrasion, 700oC/1,292F May 2013
Power Stations Opatovice Space below CC hopper CS Ash Abrasion, 700oC/1,292F May 2013
CEZ Power Station Tisova Membrane wall LAS Ash Abrasion, 700oC/1,292F Apr 2013
Trend Beijing, China Gaz tunnel oven Foam CH Fuel savings due to increased emissivity Feb 2013
Trend Beijing, China Gaz tunnel oven Foam CH Fuel savings due to increased emissivity Feb 2013

 

 

Customer Equipment Substrate Environment Date of application
Power Stations Opatovice Tank H4 in WTP CS 7% HCl Dec 2012
CEZ PS Porici LUVO Tubes CS Acid Condensate Corrosion, 140oC/284F Sept 2012
Power Stations Opatovice Hopper K3 U-bends CS Ash Abrasion, 700oC/1,292F Aug 2012
Power Stations Opatovice Hopper K2 U-bends CS Ash Abrasion, 700oC/1,292F July 2012
Power Stations Opatovice ECO II K3 tubes CS Ash Abrasion, 700oC/1,292F July 2012
CEZ PS Tisova Fluid bed FK 11 boiler High-alloyed metallic coating Ash Abrasion, 850oC/1,562F July 2012
CEZ Power Station Melnik K 11 Hopper CS Ash Abrasion, 700oC/1,292F July 2012
Power Stations Opatovice ECO K1 U-bends CS Ash Abrasion, 700oC/1,292F June 2012
CEZ HP Dvur Kralove K2 Superheater Tubes Cr/Mo Clinkering 1,200oC/2,192F June 2012
Power Stations Opatovice Hopper K1 U-bends CS Ash Abrasion, 700oC/1,292F June 2012
Power Stations Opatovice Hopper K6 U-bends CS Ash Abrasion, 700oC/1,292F May 2012
Power Stations Opatovice ECO II K5 tubes CS Ash Abrasion, 700oC/1,292F May 2012
Power Stations Opatovice Hopper K5 U-bends CS Ash Abrasion, 700oC/1,292F May 2012
Power Stations Opatovice ECO II K2 tubes CS Ash Abrasion, 700oC/1,292F May 2012
Power Stations Opatovice Hopper K4 U-bends CS Ash Abrasion, 700oC/1,292F May 2012
Power Stations Opatovice ECO K6 U-bends CS Ash Abrasion, 700oC/1,292F May 2012
Prague Incinerator Plant K3 Heatexchanger LUVO CS Corrosion by acidic condensates, 140oC/284F Apr 2012
Korund Cian, Dzerzhinsk, Russia Gas furnace PYR Protection against defibrilation, 1,200oC/2,192F March 2012

 

Customer Equipment Substrate Environment Date of application
United Energy PS Komorany Fluid boiler superheater's tubes Cr/Mo Sand&coal abrasion, up to 900oC/1,652F Sept 2011
CEZ PS Tisova Fluid bed boiler High-alloyed metallic coating Ash Abrasion, 850oC/1,562F Aug 2011
CEZ Heating Plant Porici Tubes LUVO CS Corrosion by acidic condensates, 140oC/284F Aug 2011
Prague Incinerator Plant Heatexchanger LUVO CS Corrosion by acidic condensates, 140oC/284F July 2011
Power Stations Opatovice Hopper K4 U-bends CS Ash Abrasion, 700 oC/1,292F July 2011
Heating Plant DALKIA Prerov K2 combusting chamber RC Clinkering July 2011
Lovochemie Heatexchanger E3310 SS Corrosion by concentrated HNO3, 225oC/437F June 2011
Power Stations Opatovice K6 hopper - boiling part CS Ash Abrasion, 700 oC/1,292F June 2011
Power Stations Opatovice ECO K4 U-bends CS Ash Abrasion, 700 oC/1,292F June 2011
Power Stations Opatovice Hopper & ECO K5 U-bends CS Ash Abrasion, 700 oC/1,292F May 2011
Power Stations Opatovice Hopper & ECO K8 U-bends CS Ash Abrasion, 700 oC/1,292F May 2011
Power Stations Opatovice Hopper K3 U-bends CS Ash Abrasion, 700 oC/1,292F Apr 2011
Power Stations Opatovice Hopper K2 U-bends CS Ash Abrasion, 700 oC/1,292F Apr 2011
Power Stations Opatovice ECO II K2 tubes CS Ash Abrasion, 700 oC/1,292F Apr 2011
Power Stations Opatovice Hopper K1 U-bends CS Ash Abrasion, 700 oC/1,292F Apr 2011

 

Customer Equipment Substrate Environment Date of application
Energy Centrum Jindrichuv Hradec Steam biomass boiler LAS, RB Clinkering Oct 2010
CEZ PS Tisova Fluid bed boiler's combusting chamber High-alloyed metallic coating Ash Abrasion, 850oC/1,562F Oct 2010
Pague Heating Comp. (EMe I) Superheater PP IV K1 CS Clinkering Sept 2010
EGT Sevis Ltd Retort SS High Temperature Corrosion Aug 2010
ATEKO Cyclone CrMo Abrasion0, 400oC/752F Aug 2010
CEZ HP Dvur Kralove Combustion chamber K2 Refractory Abrasion Aug 2010
CEZ PS Melnik K11 hopper, burners CS Clinkering July 2010
Pague Heating Comp. (EMe I) Superheater PP IV K2 Cr/Mo Clinkering July 2010
Power Stations Opatovice ECO II K2 U-bends CS Ash Abrasion, 700 oC/1,292F July 2010
Power Stations Opatovice  Hopper K2 U-bends LAS Ash Abrasion, 700 oC/1,292F July 2010
Power Stations Opatovice ECO II K1 tubes CS Waste gases abrasion, 700 oC/1,292F June 2010
CEZ PS Melnik Superheater PP IV K4 Cr/Mo Clinkering June 2010
Power Stations Opatovice ECO II K6 tubes CS Waste gases abrasion, 700 oC/1,292F May 2010
Power Stations Opatovice Hopper K5 U-bends CS Ash Abrasion, 700 oC/1,292F May 2010
Power Stations Opatovice Hopper K6 U-bends CS Ash Abrasion, 700 oC/1,292F May 2010
TERMIZO Liberec Tube wall fluid bed waste incinerator LAS Abrasion Apr 2010
CEZ PS Porici Steam boiler RC Clinkering Apr 2010
Caminus Praha Chimney mixers SS High Temperature Corrosion Feb 2010

 

Customer Equipment Substrate Environment Date of application
Kotle-Mont a.s. Steam boiler's combust. chamber; membrane wall LAS Clinkering, 1,200oC/2,192F Sep 2009
International Power,  PS Opatovice ECO II K5 U-bends CS Waste gases abrasion, 400oC/752F July 2009
Caminus Praha Chimney mixers SS High Temperature Corrosion July 2009
International Power,  PS Opatovice ECO II K6 U-bends CS Waste gases abrasion, 400oC/752F Jun 2009
International Power,  PS Opatovice Hopper K3 U-bends CS Ash Abrasion, 700 oC/1,292F May 2009
International Power,  PS Opatovice ECO II K2 suspension tubes CS Waste gases abrasion, 700 oC/1,292F May 2009
CEZ PS Melnik K11 hopper CS Ash Abrasion, 700 oC/1,292F May 2009
Pague Heating Comp. (EMe I) 12 pcs. LUVO (Tubes inside) CS Abrasion, 350 -180oC/662 - 356F May 2009
International Power,  PS Opatovice ECO II K4 tubes GO CS Waste gases abrasion, 700 oC/1,292F May 2009
PARAMO Pardubice Furnace H21 PYR Repair past diagnostic Mar 2009
BOSCH Thermotechnik Krnov Boiler CS Demand to improve thermal efficiency by 5% Mar 2009
Caminus Praha Chimney mixers SS High Temperature Corrosion Apr 2009

 

Customer Equipment Substrate Environment Date of application
Caminus Praha Chimney mixers SS High Temperature Corrosion Nov 2008
EGT Servis Hradec Králové Recuperator SS High Temperature Corrosion, Glass Sep 2008
International Power,  PS Opatovice Hopper Tubes (K1) CS Ash Abrasion, 700 oC/1,292F Jul 2008
International Power,  PS Opatovice Superheater Tubes (K1) Cr/Mo Clinkering, 1,200oC/2,192F Jul 2008
International Power,  PS Opatovice Burners - Boiling Tubes (K1) CS Clinkering, 1,100oC/2,012F Jul 2008
Central Sticks Libcany Boiler RC Biomass Jun 2008
International Power,  PS Opatovice Tubes ECO II - coating CS Waste gases abrasion, 700 oC/1,292F Jun 2008
Caminus Praha Chimney mixers SS High Temperature Corrosion May 2008
International Power, PS Opatovice Tubes ECO II - GO (K5) SS Ash Abrasion, 700 oC/1,292F May 2008
Paramo Pardubice Furnace H21 PYR Low Temperature Corrosion of Shell due to high sulphur content in gas Mar 2008

 

Customer Equipment Substrate Environment Date of application
Hexion Sokolov Tube wall K13 CS High Temperature Corrosion Sep 2007
Paramo Pardubice Tubes ECO - GO CS Low Temperature Corrosion, 220oC/428F Sep 2007
Dalkia Ostrava Burners - Boiling Tubes RC, CS Clinkering, 1,100oC/2,012F Aug 2007
International Power, PS Opatovice Superheater Tubes (K3) Cr/Mo Clinkering, 1,200oC/2,192F Jul 2007
International Power, PS Opatovice Tubes ECO II - GO (K5) CS Ash Abrasion, 700 oC/1,292F Jun 2007
International Power, PS Opatovice Hopper Tubes (K4) CS Ash Abrasion, 700 oC/1,292F Jun 2007
International Power, PS Opatovice Hopper Tubes (K5) CS Ash Abrasion, 700 oC/1,292F Jun 2007
Heating Plant Wroclaw (PL) Desulphurization unit CS High Temperature Corrosion Jun 2007
International Power, PS Opatovice Tubes ECO II - lower U-bend (K2) CS Waste gases abrasion, 400oC/752F May 2007
International Power, PS Opatovice Tubes ECO II - lower U-bend (K5) CS Waste gases abrasion, 400oC/752F Mar 2007
MAO Slovnaft Bratislava (SK) Burner box RC Clinkering, 1,100oC/2,012F Apr 2007

 

Customer Equipment Substrate Environment Date of application
Prague Incinerator Plant Burner wall RC Clinkering, 1,100oC/2,012F Dec 2006
Heating Plant Wroclaw (PL) Desulphurization unit LAS High Temperature Corrosion Oct 2006
International Power, PS Opatovice Superheater Tubes (K3) Cr/Mo Clinkering, 1,200oC/2,192F Aug 2006
International Power, PS Opatovice Tubes ECO II (K3) CS Waste gases abrasion, 700 oC/1,292F Aug 2006
International Power, PS Opatovice Hopper Tubes (K3) CS Ash Abrasion, 700 oC/1,292F Aug 2006
International Power, PS Opatovice Burners - Boiling Tubes (K3) Cr/Mo Clinkering, 1,100oC/2,012F Aug 2006
Pague Heating Comp. (EMe I) Fan wheel box SC Abrasion, 200oC/392F Aug 2006
MAO Slovnaft Bratislava (SK) Burner box RC Clinkering, 1,100oC/2,012F Jul 2006
Dalkia Ostrava Burners - Boiling Tubes RC, Cr/Mo Clinkering, 1,100oC/2,012F Jun 2006
International Power, PS Opatovice Tubes ECO II (K1) CS Waste gases abrasion, 700 oC/1,292F Jun 2006
International Power, PS Opatovice Hopper Tubes (K1) CS Ash Abrasion, 700 oC/1,292F Jun 2006
International Power, PS Opatovice Tubes ECO II (K4) CS Waste gases abrasion, 700 oC/1,292F May 2006
International Power, PS Opatovice Hopper Tubes (K4) CS Ash Abrasion, 700 oC/1,292F May 2006
Pague Heating Comp. (EMe I) LUVO Tubes CS Abrasion, 350 -180oC/662 - 356F May 2006
International Power, PS Opatovice Hopper Tubes (K5) CS Ash Abrasion, 700 oC/1,292F May 2006
International Power, PS Opatovice Burners - Boiling Tubes (K6) Cr/Mo Clinkering, 1,100oC/2,012F May 2006
Synthesia - Heating Plant Mixing T-tube CS Coal powder abrasion, 250oC/482F Apr 2006

 

Customer Equipment Substrate Environment Date of application
International Power, PS Opatovice Hopper Tubes (K3) CS Ash Abrasion, 700 oC/1,292F Nov 2005
Prague Incinerator Plant Tubes ECO LAS Waste gases abrasion, 700 oC/1,292F Aug 2005
Prague Incinerator Plant Burner wall RC Clinkering, 1,100oC/2,012F Aug 2005
UE Novosedlice Cyklone LAS Abrasion, 350oC/662F Aug 2005
Energetika Kladno Combustion chamber - Tube wall CS Waste gases abrasion, 1,100oC/2,012F Aug 2005
Pague Heating Comp. (EMe I) Tubes LUVO CS Abrasion, 350 -180oC/662 - 356F Jul 2005
MAO Slovnaft Bratislava (SK) Burner box RC Clinkering, 1,100oC/2,012F Jul 2005
Heating Plant Strakonice Coal Powder Silo CS Abrasion, Coal blazing Jul 2005
International Power, PS Opatovice Tubes ECO II (K6) CS Waste gases abrasion, 700 oC/1,292F Jun 2005
United Energy PS Novosedlice Cyklone LAS Abrasion, 350oC/662F Jun 2005
United Energy PS Komorany Fluid boiler nozzles (K1) SS Sand&coal abrasion, up to 900oC/1,652F May 2005
Synthesia - Heating Plant Mixing T-tube SS Coal Abrasion, 250oC/482F Apr 2005
United Energy PS Komorany Fluid boiler nozzles (K7) SS Fluid bed abrasion, 1,100oC/2,012F Apr 2005

 

Customer Equipment Substrate Environment Date of application
MAO Slovnaft Bratislava (SK) Combustion chamber - Ethylene unit Foam CH Thermal losses Dec 2004
Heating Plant Strakonice ECO II, ECO I, Burner box, Fan wheel CS, RC Abrasion, Clinkering Sep 2004
International  Power, PS Opatovice Tubes ECO II (K6) CS Waste gases abrasion, 700 oC/1,292F Sep 2004
SVZ Schwarze Pumpe (Ger.) Combustion chamber - upper side SiC, SS Clinkering, 1,300oC/2,372F Sep 2004
International Power, PS Opatovice Tubes ECO II (K2) CS Waste gases abrasion, 700 oC/1,292F Aug 2004
United Energy PS Novosedlice Combustion chamber RC Clinkering, 1,000oC/1,832 Aug 2004
Energetika Kladno Combustion chamber - Tube wall CS Waste gases abrasion, 1,100oC/2,012F Aug 2004
Prague Incinerator Plant Tubes ECO LAS Waste gases abrasion, 700 oC/1,292F Jul 2004
Heating Plant Strakonice ECO II, ECO I, heating box, fan wheel CS, RC Abrasion, Clinkering Jul 2004
United Energy PS Komorany Fluid boiler nozzles on site (K4) SS Sand&coal abrasion, up to 900oC/1,652F Jul 2004
International Power, PS Opatovice Tubes ECO II (K6) CS Waste gases abrasion, 700 oC/1,292F Jun 2004
Prague Incinerator Plant Burner wall RC Clinkering, 1,100oC/2,012F Jun 2004
Energetika Kladno Burner box RC Clinkering, 1,100oC/2,012F Jun 2004
Energoaqua Roznov pod Radhostem Burner wall RC/CH Clinkering, 1,100oC/2,012F Jun 2004
International Power, PS Opatovice Tubes ECO II (K5) CS Waste gases abrasion, 700 oC/1,292F Jul 2004
United Energy PS Komorany Fluid boiler nozzles on site (K4) SS Sand&coal abrasion, up to 900oC/1,652F May 2004
International Power, PS Opatovice Tubes ECO II (K5) CS Waste gases abrasion, 700 oC/1,292F May 2004
Synthesia Pardubice - Heating Plant Mixing T-tube SS Coal powder abrasion, 250oC/482F Apr 2004
United Energy PS Komorany Fluid boiler nozzles SS Fluid bed abrasion, 1100oC/2,012F Apr 2004

 

Customer Equipment Substrate Environment Date of application
RIOS Valasské Mezirící Sulfuric Acid condenser ARC 70% H2SO4, 260oC/500F Oct 2003
United Energy PS Novosedlice Cyklone LAS Abrasion, 350oC/662F Oct 2003
Power Station Detmarovice 4 different places LAS Black coal abrasion, up to 1,200oC/2,192F Oct 2003
International Power PS Opatovice Steam boiler K 5, nose-pieces and hooks Cr/Mo Ashes' abrasion, 460-650oC/860-1,202F Sep 2003
CD DKV Ceská Trebová Steam boiler's combust. chamber; membrane wall LAS Clinkering, 1,200oC/2,192F Sep 2003
Biomac Vetrní Pulp chips' combustion boiler RC Clinkering, 900oC/1,652F Sep 2003
Burwitz CZ ASEA Exhaust Cover CS Above melt, 1,400oC/2,552F Aug 2003
Harpen Náchod Steam boiler,  burners RC Ashes' abrasion, clinging,1,200oC/2,192F Aug 2003
United Energy PS Komorany Fluid bed boiler 8 - disc nozzels SS Sand&coal abrasion, up to 900oC/1,652F Aug 2003
Sokolovská uhelná Vresová Boiler K3, gas burners' inlet RC Clinkering, 1,200oC/2,192F Aug 2003
United Energy PS Komorany luid bed boiler 3 - disc nozzels SS Sand&coal abrasion, up to 900oC/1,652F Jul 2003
Zilinská Heating Plant Steam boiler,  burners RC Ashes' abrasion, clinging, 1,200oC/2,192F Jun 2003
United Energy PS Komorany Fluid bed boiler 7 - disc nozzels SS Sand&coal abrasion, up to 900oC/1,652F Jun 2003
KORAMO, a.s. Steam boiler,  burners RC Ashes' abrasion, clinging, 1,200oC/2,192F Jun 2003
ENERGOTRANS, a.s. Stack gas blower's blades Cr/Mo Ashes' abrasion, 300oC/572F Jun 2003
International Power PS Opatovice Steam boiler K 6, ECO II tubes Cr/Mo Ashes' abrasion, 460-650oC/860-1,202F Jun 2003
International Power PS Opatovice Steam boiler K 3, ECO II tubes Cr/Mo Ashes' abrasion, 460-650oC/860-1,202F May 2003
International Power PS Opatovice Steam boiler K 2, ECO II tubes Cr/Mo Ashes' abrasion, 460-650oC/860-1,202F May 2003
IROMEZ Pelhrimov Biomass combust. boiler, heatexchanger's tubes Cr/Mo Clinging in tubes' mouth, 600-900oC/1,112-1,652F Apr 2003
ESAB Vamberk Melting furnaces cover Ganister Above the melt, 1,650oC/3,000F Mar 2003
Synthesia Heating Plant Steam boiler, mixing pieces CS cast Black coal, 310oC/590F Mar 2003
Zilinská Heating Plant Steam boiler, hopper, burners RC Abrasion, clinging, 1,200oC/2,192F Mar 2003
IVITAS Converter's Hood LAS Backsplashing steel and slag, 1,500oC/2,732F Feb 2003

 

Customer Equipment Substrate Environment Date of application
Heating Plant Ceske Budejovice Boiler, coal burners combin. Clinkering Aug 2002
Heating Plant DALKIA Olomouc Fluid bed boiler RB Abrasion from fluid bed Jul 2002
International Power PS Opatovice Boiler K 1, nozzle LAS Ashes' abrasion, 460-650oC/860-1,202F Jul 2002
Power Station Melnik Boiler K11, duct 3 CS Ashes' abrasion, 200-250oC/392-482F Jul 2002
Sokolovská uhelná Vresová Boiler, gas burners' gates RC Clinkering, 1,200oC/2,192F Jun 2002
International Power PS Opatovice Armouring - powder coal supply, boiler #2 LAS Coal powder abrasion, up to 1,000oC/1,832F Jun 2002
International Power PS Opatovice Superheater's tube sheet of boiler # 2 LAS Abrasion, up to 1,300oC/2,372F Jun 2002
International Power PS Opatovice Superheater's waste gases' breaker of boiler #2 RC Abrasion, up to 1,300oC/2,372F Jun 2002
Heating Plant Ústí nad Labem Boiler's combusting chamber, coal dryers gates CH Clinkering May 2002
Power Station Prunérov Boiler's combusting chamber spoiling grate RC Abrasion and falling clinckers' impact May 2002

 

Customer Equipment Substrate Environment Date of application
Galena Opava Gas Boiler's Steam Superheater LAS Impact wall, 800oC/1,472F Oct 2001
International Power PS Opatovice Boiler K 6 Cr/Mo, RC Ashes' abrasion, 460-650oC/860-1,202F Sep 2001
Power Station Trinec Fluid bed boiler, membrane wall LAS Abrasion, 900oC/1,652F Sep 2001
Heating Plant Tábor Boiler, gas burners' gates RC, Sibral Clinkering, 1,200oC/2,192F Aug 2001
Sokolovská uhelná Vresová Boiler, gas burners' gates RC Clinkering, 1,200oC/2,192F Jul 2001
Heating Plant Ústí nad Labem Boiler's combusting chamber, membrane wall LAS Clinkering Jul 2001
United Energy PS Komorany Fluid bed boiler: disc nozzels SS Sand&coal abrasion, up to 900oC/1,652F Jun 2001
Hospital Benesov Incinerator's combusting chamber RC Clinkering, 1,600oC/2,912F Jun 2001
Power Station Trinec Fluid bed boiler, membrane wall LAS Abrasion, 900oC/1,652F May 2001
MST Energomont Boiler, burners' gates RC Deposits&clinkering, 1,000oC/1,832F May 2001
Power Station Turow, Poland Fluid bed boiler's combusting chamber LAS, RC Abrasion, 800oC/1,472F Apr 2001
Heating Plant Rýmarov Steam boiler CH Clinkering, 1,100oC/2,012F Apr 2001
Hospital Benesov Incinerator's combusting chamber RC Clinkering, 1,600oC/2,912 Apr 2001
Heating Plant Rýmarov Steam boiler CH Clinkering, 1,100oC/2,012F Feb 2001
Power Station CEZ Ledvice 60 pcs burners SS Coal powder abrasion, 350oC/662F Jan 2001

 

Customer Equipment Substrate Environment Date of application
International Power PS Opatovice Steam boiler's ECO II Cr/Mo, CH Ashes' abrasion, 460-650oC/860-1,202F Dec 2000
Heating Plant Bruntál Steam boiler SS Creep, 1,100oC/2,012F Oct 2000
Paramo Pardubice Power plant: boiler CH Clinkering, 1,200oC/2,192F Sep 2000
United Energy PS Komorany Fluid bed boiler: nozzels SS Sand&coal abrasion, up to 900oC/1,652F Sep 2000
SAKO Brno Boiler in waste combustion unit RC Clinkering, 1,200oC/2,192F Sep 2000
Iromez Pelhrimov 2 leight fuel oil boilers CH Clinkering, 1,200oC/2,192F Sep 2000
ASSI Domän Stúrovo Regeneration boiler RC Clinkering, 1,200oC/2,192F Sep 2000
Spolana Neratovice Caprolactame plant: Sulphur combustion's oven CH Gaseous SO2, 1,400oC/2,552F Aug 2000
International Power PS Opatovice Superheater's waste gases' breaker of boiler # 3 RC Abrasion, up to 1,300oC/2,372F Aug 2000
Sokolovská uhelná Vresová Incinerator RC Abrasion, 1,200oC/2,192F Aug 2000
International Power PS Opatovice Armouring - powder coal supply LAS Abrasion, up to 1,000oC/1,832F Aug 2000
Kávoviny Pardubice Roasting furnace CH Waste gases, 1,300oC/2,372F Jul 2000
Skoda Energo Mladá Boleslav Fluid bed boiler Cr/Mo, CH Abrasion, 900oC/1,652F Jul 2000
International Power PS Opatovice Superheater's tube sheet of boiler # 3 Cr/Mo Abrasion, up to 1,300oC/2,372F Jul 2000

 

Customer Equipment Substrate Environment Date of application
Heating Plant Liberec Gaz boiler CH 1,200oC/2,192F Dec 1999
United Energy PS Komorany Fluid bed boiler: nozzels - test SS Sand&coal abrasion, up to 900oC/1,652F Oct 1999
International Power PS Opatovice Armouring - powder coal supply LAS, RC Coal powder abrasion, up to 1,000oC/1,832F Sep 1999
International Power PS Opatovice Superheater's tube sheet of boiler # 4 Cr/Mo Abrasion, up to 1,300oC/2,372F Sep 1999
International Power PS Opatovice Superheater's waste gases' breaker of boiler # 4 RC Abrasion, up to 1,300oC/2,372F Sep 1999
Spolana Neratovice Sulphuric acid plant: collecting main - test SS 98-99% H2SO4, 90oC/194F Sep 1999
Spolana Neratovice Sulphuric acid plant: mixing tank - test SS 98-99% H2SO4, 90oC/194F Sep 1999
Spolana Neratovice Sulphur combustion's oven - test CH Gaseous SO2, clinkering, 1,200oC/2,192F Aug 1999
PRECHEZA Prerov Sulphur combustion's oven K - test CH Gaseous SO2, clinkering, 1,200oC/2,192F Aug 1999
PRECHEZA Prerov Sulphur combustion's oven S1 - test CH Gaseous SO2, clinkering, 1,200oC/2,192F Aug 1999
Léciva Praha Pyrolyzer in destruction unit CH, RC Chemical and municipal wastes, 800oC Aug 1999
PRECHEZA Prerov Rotary kiln B by titanium white production CH H2SO4, TiO2, 470oC/878F Aug 1999
PRECHEZA Prerov Ilmenite's pyrolyzer RC Waste gases, 1,600oC/2,912F Aug 1999
PRECHEZA Prerov Rotary kiln A by titanium white production CH H2SO4, TiO2, 470 - 950oC/878 - 1,742F Aug 1999
Chemopetrol Litvínov Petrochemical oven BA 10 Foam CH Crude oil fractions combustion, 900oC/1,652F Jul 1999
Sokolovská uhelná Vresová Incinerator LICHEP PYR Waste gases combustion, 1,500oC/2,732F Jul 1999
PRECHEZA Prerov Sulphuric acid absorbtion tower APC 75% H2SO4, 150oC/302F Jul 1999
Chemopetrol Litvínov Petrochemical oven BA 107 RC Crude oil fractions combustion, 1,200oC/2,192F Jul 1999
PRECHEZA  Prerov Rotary kiln A by titanium white production CH H2SO4, TiO2, 470oC Jun 1999
Paramo Pardubice Incinerator CH, RC Acidic condensates, 800oC/1,472F Mar 1999
SBK Ostrava Gaz crucible furnace CH Flame, slag, 1,300oC/2,372F Jan 1999
International Power PS Opatovice Armouring - powder coal supply CH, CS Coal powder abrasion, up to 1,200oC/2,192F Jul 1998